Grade | Ni+Co | Cu | Si | Mn | C | Mg | S | P |
N4 | 99.8 | 0.015 | 0.03 | 0.002 | 0.01 | 0.01 | 0.001 | 0.001 |
N6 | 99.6 | 0.10 | 0.10 | 0.05 | 0.10 | 0.10 | 0.005 | 0.002 |
Ni201 | ≥99.0 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.02 | / | ≤0.01 | / |
Ni200 | ≥99.2 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.15 | / | ≤0.01 | / |
Physical Data | |||||
Density | Specific Heat | Electrical Resistivity | Melting Point | Thermal Conductivity | Mean Coeff Thermal Expansion |
8.89g/cm3 | 0.109(456 J/kg.ºC) | 0.096×10-6ohm.m | 1435-1446ºC | 70.2 W/m-K | 13.3×10-6m/m.ºC |
Typical Mechanical Properties | |||||
Mechanical Properties | Tensile Strength | Yield Strength | Elongation | Standard | |
Nickel 200 | 462 Mpa | 148 Mpa | 47% | ASTM B161/B163/B725/B751 |