Filter | Weight (g/m2) | Thickness (mm) |
Air permeability (m3/m2·min) | Tensile Strength (N/5×20cm) |
Tensile elongation (%) | Working Temperature (℃) |
Finishing Treatment | ||
Polyester+Plyester Staple Scrim | 450 | 1.6 | 18 | ≥900 | ≥1200 | ≤25 | ≤45 | ≤130 | Singeing, Calendering, Heating, Coating |
500 | 1.8 | 15 | ≥900 | ≥1200 | ≤25 | ≤45 | ≤130 | ||
550 | 2 | 13 | ≥1800 | ≥1800 | ≤10 | ≤10 | ≤130 | ||
600 | 2.2 | 12 | ≥900 | ≥1200 | ≤25 | ≤35 | ≤130 | ||
POlyester+Plyester Filament Scrim | 400 | 1.4 | 21 | ≥1000 | ≥1250 | ≤25 | ≤45 | ≤130 | |
450 | 1.55 | 18 | ≥1000 | ≥1300 | ≤25 | ≤45 | ≤130 | ||
500 | 1.75 | 15 | ≥1100 | ≥1350 | ≤25 | ≤45 | ≤130 | ||
550 | 1.95 | 13 | ≥1100 | ≥1350 | ≤25 | ≤45 | ≤130 | ||
600 | 2.15 | 12 | ≥1150 | ≥1400 | ≤25 | ≤45 | ≤130 |