EN10025 S275JR Chemical Composition(%) and Mechanical Performance | ||||||||
Thickness | C | Mn | P | S | Cu | N | Tensile Strength MPA |
Yield Strength MPA |
≤16mm | ≤0.21 | ≤1.50 | ≤0.035 | ≤0.035 | ≤0.55 | ≤0.012 | 430-580 | ≥275 |
16mm-40mm | ≤0.21 | ≤1.50 | ≤0.035 | ≤0.035 | ≤0.55 | ≤0.012 | 430-580 | ≥275 |
>40mm | C≤0.22 | ≤1.50 | ≤0.035 | ≤0.035 | ≤0.55 | ≤0.012 | 430-580 | ≥275 |